Current research projects

Image Industry 4.0 membrane heat and mass exchanger (i-MWÜ4.0)
Image Multifunctional electronic modules for cryogenic applications
Image Cool Up
Image In-situ investigation concerning the swelling behaviour of polymer materials under elevated pressures and temperatures
Image Solar Cooling
Image Pulse-Tube-Refrigerator with sealed compressor
Image 3D - Air flow sensor
Image Cold meter
Image Investigation of coolants
Image Ice Slurry Generation
Image Service offer for Leak Detection and Tightness Test
Image Tribological investigations of oil-refrigerant-material-systems
Image Modular storage system for solar cooling
Image Investigation according to DIN EN ISO 14903
Image Characterisation of Superconductors in Hydrogen Atmosphere
Image Cryogenic liquid piston pumps for cold liquefied gases like LIN, LOX, LHe, LH2, LNG, LAr

You are here:   /  Home


Investigation of material-dependent parameters

Industry and R&D

Gunar Schroeder

+49-351-4081-5129

Investigation of the permeation behavior

Permeation is the penetration of solid matter by another substance. The driving force for this is a gradient of the chemical potential of the permeate. In practice, this gradient is replaced by a measurable quantity such as the pressure gradient. The permeability of a material depends on the surface temperature and is usually specified with the unit \( \frac{\mu g}{cm^2\:min} \)

Without external influences, the permeate always moves in the direction of the lower concentration or the lower partial pressure. For theoretical consideration, permeation can be divided into three sections across the solid:

  • Sorption, for example, a gas is absorbed at the surface of the solid
  • Diffusion, this gas diffuses through the solid through molecular gaps towards the surface with a lower gas concentration
  • Desorption, the gas is released again from this surface

The experimental setup to investigate this process, see the following figures, essentially consists of a sample chamber. The sample is mounted with a seal or against a sealing surface. A test gas with a defined overpressure is applied to the volume on the "left" of the sample. The volume to the "right" of the sample is connected to a detector. The pressure on both sides of the sample, the temperatures and the gas flow rate are measured over a longer period of time (24 - 48 h).

Parameter Sample limits
materials plastics, metals
dimensions, diameter, and wall thickness 58 ... 60 mm, 1 ... 3 mm
other dimensions on request
pressure difference up to 10 bar (145 psi)
temperature range room temperature, other conditions on request
test gas helium or hydrogen
detector measuring range up to \(10^{-9} \frac{mbar\:l}{s} \), optional with calibration

 